<div>Dear all,</div><div> </div><div>I have a question, regarding the use of DFT+U for the material like VSe2 (TMDs). This is a ferromagnetic metal in the bulk form, according to the literature. Plain DFT (PBE) does reproduce this behavior. However, in some papers I see that people apply DFT+U to V atoms.</div><div>I'm curious to know is it really necessary. Band gap is not an issue here. I even tried to use the value provided in the papers, and lattice parameters were even worse with DFT+U than without. Magnetic moment on V jumped from 0.6 (without U) to 1.3 (with U), which is expected.</div><div> </div><div>What would be the indicator that it is quite important to apply U correction for materials?</div><div> </div><div>Thanks,</div><div> Sergey</div><div>University of South Florida</div><div> </div>